A high entropy silicide by reactive spark plasma sintering Y Qin, JX Liu, F Li, X Wei, H Wu, GJ Zhang Journal of Advanced Ceramics 8 (1), 148-152, 2019 | 275 | 2019 |
Residual stresses in composite materials MM Shokrieh Woodhead publishing, 2014 | 155* | 2014 |
The strength of Al2O3/SiC nanocomposites after grinding and annealing HZ Wu, CW Lawrence, SG Roberts, B Derby Acta materialia 46 (11), 3839-3848, 1998 | 114 | 1998 |
Subsurface damage analysis by TEM and 3D FIB crack mapping in alumina and alumina/5vol.% SiC nanocomposites HZ Wu, SG Roberts, G Möbus, BJ Inkson Acta Materialia 51 (1), 149-163, 2003 | 104 | 2003 |
Residual stress and subsurface damage in machined alumina and alumina/silicon carbide nanocomposite ceramics H Wu, SG Roberts, B Derby Acta materialia 49 (3), 507-517, 2001 | 87 | 2001 |
陶瓷料浆稳定分散进展 王瑞刚, 吴厚政 陶瓷学报 20 (1), 35-40, 1999 | 71 | 1999 |
High-entropy silicide ceramics developed from (TiZrNbMoW) Si2 formulation doped with aluminum Y Qin, JC Wang, JX Liu, XF Wei, F Li, GJ Zhang, C Jing, J Zhao, H Wu Journal of the European Ceramic Society 40 (8), 2752-2759, 2020 | 50 | 2020 |
Microstructure of friction surface developed on carbon fibre reinforced carbon–silicon carbide (Cf/C–SiC) Y Wang, H Wu Journal of the European Ceramic Society 32 (12), 3509-3519, 2012 | 50 | 2012 |
Friction surface evolution of carbon fibre reinforced carbon/silicon carbide (Cf/C-SiC) composites Y Wang, H Wu Journal of the European Ceramic Society 30 (15), 3187-3201, 2010 | 50 | 2010 |
Residual stress distributions around indentations and scratches in polycrystalline Al2O3 and Al2O3/SiC nanocomposites measured using fluorescence probes HZ Wu, SG Roberts, B Derby Acta materialia 56 (1), 140-149, 2008 | 48 | 2008 |
Mesoscopic structure features in synthetic graphite B März, K Jolley, TJ Marrow, Z Zhou, M Heggie, R Smith, H Wu Materials & Design 142, 268-278, 2018 | 45 | 2018 |
Contact damage of silicon carbide ceramics with different grain structures measured by Hertzian and Vickers indentation J Wade, S Ghosh, P Claydon, H Wu Journal of the European Ceramic Society 35 (6), 1725-1736, 2015 | 44 | 2015 |
Friction performance of carbon/silicon carbide ceramic composite brakes in ambient air and water spray environment G Bian, H Wu Tribology International 92, 1-11, 2015 | 43 | 2015 |
Synergetic roles of ZrC and SiC in ternary ZrB2–SiC–ZrC ceramics HL Liu, GJ Zhang, JX Liu, H Wu Journal of the European Ceramic Society 35 (16), 4389-4397, 2015 | 42 | 2015 |
Friction and surface fracture of a silicon carbide ceramic brake disc tested against a steel pad G Bian, H Wu Journal of the European Ceramic Society 35 (14), 3797-3807, 2015 | 41 | 2015 |
Plasma augmented laser welding of 6 mm steel plate PT Swanson, CJ Page, E Read, HZ Wu Science and Technology of Welding and Joining 12 (2), 153-160, 2007 | 38 | 2007 |
Shock-wave induced compressive stress on alumina ceramics by laser peening P Shukla, R Crookes, H Wu Materials & Design 167, 107626, 2019 | 34 | 2019 |
A ReaXFF carbon potential for radiation damage studies R Smith, K Jolley, C Latham, M Heggie, A Van Duin, D van Duin, H Wu Nuclear Instruments and Methods in Physics Research Section B: Beam …, 2017 | 34 | 2017 |
Surface engineering alumina armour ceramics with laser shock peening P Shukla, S Robertson, H Wu, A Telang, M Kattoura, S Nath, SR Mannava, ... Materials & Design 134, 523-538, 2017 | 30 | 2017 |
Mechanical behaviour of the constituents inside carbon-fibre/carbon-silicon carbide composites characterised by nano-indentation A Leatherbarrow, H Wu Journal of the European Ceramic Society 32 (3), 579-588, 2012 | 28 | 2012 |