Aluminium matrix composites: Challenges and opportunities MK Surappa Sadhana 28, 319-334, 2003 | 1712 | 2003 |
Preparation and properties of cast aluminium-ceramic particle composites MK Surappa, PK Rohatgi Journal of materials science 16, 983-993, 1981 | 423 | 1981 |
Fabrication and characterisation of pure magnesium-30 vol.% SiCP particle composite RA Saravanan, MK Surappa Materials Science and Engineering: A 276 (1-2), 108-116, 2000 | 402 | 2000 |
Wear and abrasion of cast Al-alumina particle composites MK Surappa, SV Prasad, PK Rohatgi Wear 77 (3), 295-302, 1982 | 324 | 1982 |
Tribological behavior of Al–Si–SiCp composites/automobile brake pad system under dry sliding conditions RK Uyyuru, MK Surappa, S Brusethaug Tribology international 40 (2), 365-373, 2007 | 278 | 2007 |
Dry sliding wear of fly ash particle reinforced A356 Al composites MK Surappa Wear 265 (3-4), 349-360, 2008 | 264 | 2008 |
Synthesis of fly ash particle reinforced A356 Al composites and their characterization MK Surappa Materials Science and Engineering: A 480 (1-2), 117-124, 2008 | 261 | 2008 |
Microstructure evolution during solidification of DRMMCs (Discontinuously reinforced metal matrix composites): State of art MK Surappa Journal of Materials Processing Technology 63 (1-3), 325-333, 1997 | 236 | 1997 |
Effect of macro-porosity on the strength and ductility of cast Al 7Si 0.3 Mg alloy MK Surappa, E Blank, JC Jaquet Scripta Metallurgica 20 (9), 1281-1286, 1986 | 191 | 1986 |
Effect of reinforcement volume fraction and size distribution on the tribological behavior of Al-composite/brake pad tribo-couple RK Uyyuru, MK Surappa, S Brusethaug Wear 260 (11-12), 1248-1255, 2006 | 184 | 2006 |
Dry sliding wear of A356-Al-SiCp composites BNP Bai, BS Ramasesh, MK Surappa Wear 157 (2), 295-304, 1992 | 167 | 1992 |
Abrasive wear of cast aluminium alloy-zircon particle composites A Banerji, SV Prasad, MK Surappa, PK Rohatgi wear 82 (2), 141-151, 1982 | 143 | 1982 |
Dry sliding wear behavior of Al2O3 fiber reinforced aluminum composites Y Iwai, T Honda, T Miyajima, Y Iwasaki, MK Surappa, JF Xu Composites science and technology 60 (9), 1781-1789, 2000 | 135 | 2000 |
Cast aluminum alloys containing dispersions of zircon particles A Banerji, MK Surappa, PK Rohatgi Metallurgical Transactions B 14, 273-283, 1983 | 124 | 1983 |
Effect of sliding speed on wear behaviour of A356 Al-30 wt.% SiCp MMC A Ravikiran, MK Surappa wear 206 (1-2), 33-38, 1997 | 118 | 1997 |
The UPAL process: a direct method of preparing cast aluminium alloy-graphite particle composites BP Krishnan, MK Surappa, PK Rohatgi Journal of materials science 16, 1209-1216, 1981 | 115 | 1981 |
Dry sliding wear of A356-Al-SiC [sub p] composites BN Pramila Bai, BS Ramasesh, MK Surappa Wear;(Switzerland) 157 (2), 1992 | 110 | 1992 |
Corrosion behaviour of silicon carbide particle reinforced 6061/Al alloy composites MSN Bhat, MK Surappa, HVS Nayak Journal of materials science 26, 4991-4996, 1991 | 96 | 1991 |
Heat diffusivity criterion for the entrapment of particles by a moving solid-liquid interface MK Surappa, PK Rohatgi Journal of Materials Science 16, 562-564, 1981 | 95 | 1981 |
The effect of SiC particles on the size and morphology of eutectic silicon in cast A356/SiCp composites S Nagarajan, B Dutta, MK Surappa Composites Science and technology 59 (6), 897-902, 1999 | 92 | 1999 |